Thermal Paste Stencil Printing and Jetting Compared
Print or Dispense: Why Thermal Paste Wins the Thin Joint
Stencil printing vs jet dispensing · 20–40 µm bond line · 1.2–6.5 W/m·K
Pads, phase-change films, potting compounds and adhesives all do one thing well: fill space. A thermal paste does the opposite — it removes space. That single difference decides which process you specify, and whether the joint costs 0.3 K or 5 K.
01Every alternative begins by adding a layer
A thermal interface is a resistor: R = t / k, thickness over conductivity. Nothing else in that formula matters. A 0.5 mm pad at 5 W/m·K is 1.0 °C·cm2/W no matter how good the polymer is, and a 1.0 mm pad at 3 W/m·K is 3.3 °C·cm2/W. A phase-change film starts near 0.15 °C·cm2/W only after it has been held above its melt point long enough to wet out, which in a 25 W module that never exceeds 60 °C simply does not happen. A potting compound at 1 W/m·K is 10 °C·cm2/W at 1 mm, and it is there to protect the assembly, not to cool it. A thermally filled adhesive adds a structural bond and 1.5–2.5 °C·cm2/W at 150 µm, and it cannot be reworked.
A thermal paste is the only class of material whose thickness is set by the process rather than by the part: 20 to 40 µm is normal, 50 µm is already a mistake, and the joint can be as thin as 10 µm where the clamp is stiff. That is why a paste at 0.080 °C·cm2/W beats a 0.5 mm pad by a factor of twelve on the same footprint, and it is the only thermal interface material that gets better as the clamp gets stiffer.
02What stencil printing gives the paste
Stencil printing is the process that makes the thin joint repeatable at volume. A 0.1 mm stainless stencil with 80 % aperture coverage deposits 5.4 mg/cm2, and because the paste is thixotropic it holds that profile until the clamp closes. Two rules govern the design. First, the aperture area ratio — aperture area over wall area — should stay above 0.66; below that the paste does not release cleanly and the deposit is short on one side. Second, the print parameters are narrow: 30–50 mm/s squeegee speed, 8–15 N per 100 mm of blade, 60° blade angle, and a 1–3 mm/s separation so the paste is sheared off rather than pulled into strings.
The commercial argument is as strong as the technical one. Stencil printing transfers more than 90 % of the material into the joint, runs at hundreds of units per hour, and prints every tab on a panel in one stroke, so a 12-up charger panel gets twelve identical 20 µm joints with one operator motion. A syringe dispensing twelve separate 0.4 mg shots does not; the small ones drift, and the drift is invisible until the thermal test.
Where printing stops working
Printing needs a flat, accessible surface and a panel that fits the printer. A thermal paste printed onto a 0.3 mm stepped surface, or onto a component already standing 4 mm tall, will be smeared, and a stencil that has to clear tall parts needs a window frame that adds cost. Under about 0.5 mm2 of aperture per joint, printing also stops being practical — the deposit becomes too small to release consistently, and jetting is the better answer.
03What jet dispensing gives the paste
Jet dispensing is the answer for the other half of the product range: single small parts, mixed heights, and lines that change model every shift. A piezo or pneumatic jet fires a fixed droplet volume at 200–1,000 Hz with no needle contact, so it can dose onto a 7 mm2 tab, into a pocket, or next to a component 2 mm away, and it can follow a CAD path without a fixture. Shot mass repeatability of ±10 % is achievable on a 0.5–2 mg shot once the valve is characterised, and that is the number to qualify, not the nominal: for a thermal interface material dosed in drops, repeatability is the argument.
What jetting cannot do is produce a 20 µm film over 20 cm2 in one pass. Each dot is a discrete deposit that must coalesce, and a large area dosed dot by dot costs time and leaves a wavy profile. The practical split is therefore clean: stencil printing for panels and uniform footprints, jetting for small or irregular joints and for low volume. Both thermal paste routes beat a pad wherever the joint can be made thin.
04Six materials on the same footprint
| Material | Typical thickness | Impedance (°C·cm2/W) | Pressure needed | Rework | Volume process |
|---|---|---|---|---|---|
| Thermal paste, 0.080 | 20–40 µm | 0.080 | 10–50 psi | Yes, clean and re-apply | Stencil or jet |
| Thermal paste, 0.030 | 10–25 µm | 0.030 | 30–60 psi | Yes | Stencil |
| Gap pad, 5 W/m·K | 0.5 mm | 1.0 | 10–30 psi | Yes, replace | Pick and place |
| Phase-change film | 50–100 µm | 0.15 after wet-out | 20–40 psi | Yes | Pick and place |
| Potting compound, 1 W/m·K | 1–3 mm | 10 at 1 mm | None | No | Pot or cast |
| Thermally filled adhesive | 100–200 µm | 1.5–2.5 | None, cures | No | Dispense and cure |
Read the table as a cost of thickness, not a ranking of brands; every candidate thermal interface material here is decided by thickness rather than by conductivity. Only the first two rows put less than 40 µm of thermal paste between the hot part and the spreader, and only those two can be produced by a printing or jetting process at production speed. The others are legitimate answers to a different question — a 2 mm gap, a structural bond, a housing that must be sealed.
05Stencil printing against jetting, on the line
| Criterion | Stencil printing | Jet dispensing |
|---|---|---|
| Film thickness control | Set by foil thickness, ±5 µm | Set by dot volume and coalescence, ±15 µm |
| Throughput | Whole panel in one stroke | 200–1,000 dots/s, path dependent |
| Smallest practical joint | About 0.5 mm2 aperture | 0.05 mm2 and below |
| Surface requirement | Flat, coplanar, fixture-free | Tolerates steps and mixed heights |
| Changeover | New stencil per footprint | New program, same valve |
| Material loss | Under 10 % | 5–15 %, purge dependent |
Note what the two columns share: both deposit the same thermal paste, both produce a joint an order of magnitude thinner than a pad, and both can be validated by weighing a coupon. That is the real advantage of a thermal paste over every solid-format thermal interface material — the process, not the polymer, sets the thickness, and the process can be measured.
06Five process failures worth designing out
Slump after printing. A thermal paste that flows after the squeegee leaves a thin edge and a thick centre, so the clamp closes on the centre and the edge stays dry. Thixotropy is the property that prevents it; specify slump resistance rather than viscosity alone.
Screen clogging between cycles. Thermal paste left in apertures skins over in minutes. A production stencil needs a wipe every 10–20 prints and a full clean at shift end, or the first board after a break is short of material.
Air entrapment in jetting. A droplet that carries a bubble collapses into a void, and a void in a 20 µm joint is a hot spot. Degas the cartridge, keep the valve upright, and inspect the first article under a microscope.
Oil bleed onto the surrounding board. Excess paste around a small joint migrates outward over thermal cycles and can reach a connector or a creepage path. Dose to the aperture, not to the eye, and keep 1 mm clear of anything that must stay clean.
07Grades and where they print
The TSAD Series from TOUSEN covers 1.2–6.5 W/m·K in a solvent-free, non-curing, thixotropic gray paste, with impedance from 0.201 down to 0.030 °C·cm2/W at 30 psi, specific gravity 2.5–2.9 g/cm3, screen-printable consistency, low slump and a 12-month shelf life. Selection follows the process: the thermal paste grade must be printable at the foil thickness you own, and it must hold its impedance at the clamp pressure you actually deliver.
| Grade | W/m·K | Impedance @ 30 psi (°C·cm2/W) | Density (g/cm3) | Process fit |
|---|---|---|---|---|
| TSAD60 | 1.2 | 0.201 | 2.5 | Large-area printing, low flux |
| TSAD66 | 3.5 | 0.080 | 2.7 | Standard 0.1 mm stencil, 20–40 µm |
| TSAD66-P | 4.0 | 0.070 | 2.6 | Rougher spreaders, thicker print |
| TSAD83 PLUS | 5.2 | 0.050 | 2.6 | Jetting, small high-flux tabs |
| TSAD88 PLUS | 5.2 | 0.030 | 2.9 | Stiff clamp, printed thin |
| TSAD90 | 6.5 | 0.030 | 2.7 | Panel printing, multi-tab |
| TSAD100 | 6.5 | 0.030 | 2.8 | High-conductivity, jet or print |
08Validate the process, then the part
Weigh ten coupons from the first print of every stencil and every valve setup; the mass against the theoretical 5.4 mg/cm2 tells you the bond line before anything is powered. Then run 1,000 thermal cycles, 500 hours of damp heat and an oil separation test on the paste alone, and section one unit to measure the joint at the centre and the edge. If the print is right and the clamp is right, the joint will be 20–40 µm at both points, and no pad or potting compound in the table above can match that at any price.
Thermal paste wins in stencil printing and jet dispensing for one reason: it is the only interface material whose thickness is a process variable instead of a component specification. Choose the grade by its impedance at your clamp pressure, set the foil at 0.1 mm, print a panel or jet the small parts, and control the mass rather than the appearance. The full grade table, pressure-impedance curves and print trial samples are on the TSAD Series thermal paste product page.